Source high-rigidity solid carbide end mills and drills engineered for longer tool life, faster feeds, and tight tolerances.
The mic said the hole was big enough. The pin disagreed. That gap, size versus shape, is the usual reason a structural shop starts asking about solid carbide twist drills for structural steel.
Short answer, with the limits in the same breath. On a rigid machine, a holder that really runs true, and a clamp that holds the plate still, a solid carbide twist drill will usually cut a rounder hole in A36, A572, A992, or S355 than a flexible HSS jobber, and it will often make the reamer unnecessary on bolt clearance and on many slip-fit pins. It will not hold a press fit. It will not forgive a loose spindle, a ringing plate, or a weld it was not meant to enter. And it is the wrong purchase for a magnetic drill that already knocks the corners off cobalt tools.
This page is an application note from Durable Mills. Standards and toolmaker charts are named as such. The beam formula further down is a simplified model, not a prediction of how many microns your hole will move. The bracket story is a shop pattern, not a published cutting trial. Nothing here is a substitute for the chart that belongs to the exact drill in the spindle.
Yes, for production holes in hot-rolled structural steel on equipment that can keep the tool on axis. That covers a lot of real work: CNC plate lines, beam lines, and machining centers drilling flanges, gussets, lugs, and base plates.
Structural steels in this conversation:
What makes these grades annoying is not hardness. Hot-rolled plate carries mill scale, an abrasive oxide that rounds an outer corner early. The body of the steel is soft and ductile, so a dull corner rubs, the surface work-hardens, and the exit cap bends into a burr instead of shearing off. Long chips pack a tight flute. None of that requires a “hard” steel. It requires a drill that stays sharp, stays straight, and has somewhere for the chip to go.
Suitable setup, in plain terms:
Unsuitable, even if the catalog says “for steel”:



Engineered for high-efficiency holemaking, our solid carbide drill delivers exceptional centering precision across alloy steel and cast iron. This premium solid carbide drill bit features external cooling and an m7 tolerance for smooth chip flow. Choose our solid carbide drills for rigid, high-speed CNC drilling operations.
A two-flute drill is located by two margins. If one lip sits higher than the other, that lip cuts on a larger radius and the hole goes oversize. A bench approximation, not a clause in a standard: extra diameter is on the order of twice the lip-height mismatch. Treat it as a reason to check both lips under a glass, not as a number you can stamp on a report. On a mid-size hole, IT8 is only 0.027 mm wide, so a lip mismatch around 0.01 mm is already most of that band if the rule of thumb holds.
Runout does the same job from the spindle side. The drill orbits. People like to say the hole then “goes three-sided.” Sometimes it does. A two-flute tool with radial play often settles into an odd number of lobes, three being the one inspectors learn to hate, because a two-point micrometer can miss it. ISO 12181-1 is the vocabulary for that roundness error; the symbol on a drawing sits in ISO 1101. But lobe count is not a law. Lip geometry, margin width, spindle dynamics, the steel, the clamp, and the filter on the measuring instrument all get a vote. A wandering drill can give you a sloppy oval, a three-lobe form, or a hole that is simply torn. Measure the form. Don’t assume the triangle.
Diameter is not roundness. Two-point size can pass while a plug, or the pin that actually assembles, will not enter. If the only gauge on the bench is a micrometer, you are not inspecting the failure your fitter is seeing.
Thrust bells a thin flange or a tacked bracket. The plate springs back. The hole records that movement as lobes or as an oval that changes from the first hole to the tenth, even though nobody touched the offsets. Tap the plate. If it rings, the drill is not your first problem. Clamp within about a diameter of the hole, support the exit, and bolt stacks so the layers cannot creep. Tacks at one corner and all the clamps at one end of a beam are how a clean first hole and a triangular later hole show up on the same part. In one job we looked at, nothing had changed on the tool. The beam had.
Scale sands the outer corner. After that the drill rubs. Rubbing in ductile steel raises a hard skin, the margin polishes a shiny torn wall, and the exit crown gets taller as the corner gets rounder. A coating delays that. It does not restore a lip that was ground off-center, and it does not put stiffness into a long, skinny body.
Cemented carbide and high-speed steel are not the same material with a different price. Published handbook values put tungsten carbide near 530 to 700 GPa elastic modulus. High-speed steel sits near 210 GPa, in the same neighborhood as the workpiece. Same shape, same load, the carbide bends about a third as much. That ratio is the roundness argument. Hot hardness is the tool-life argument: HSS starts to soften once the edge region is up around 550 to 600°C, and carbide still has a cutting edge well past that temperature. You can feel the difference in your hand. Carbide tooling grades are about 14 to 15 g/cm3. M2 is about 8 g/cm3.
The deflection formula is only a way to see the trend:
deflection = (force × length × length × length) / (3 × elastic modulus × second moment of area)
It is a simplified cantilever: one lateral load, a constant round section. A drill is not that bar. The flutes have already removed material, so the real second moment is lower and the absolute sag is worse than the round-bar number. Length still cubes. Twice the stickout is about eight times the deflection if nothing else changes. Modulus still sits in the denominator once, so the carbide-versus-HSS ratio remains about threefold when the shape is the same. Do not turn the formula into a predicted hole error. Use it when someone wants to run a long drill “because it was in the crib.”
Cobalt HSS (M35, M42) is still steel. It holds hardness a bit further than plain HSS and it is tougher than carbide, which is why it survives portable machines that chip carbide on the first bump. It does not match carbide stiffness or carbide speed on a rigid CNC. Sandvik Coromant states that solid carbide drills can reach hole tolerances on the order of IT8. Kennametal’s Joe Slusarcyk told MSC the same thing with the condition attached: good setup, minimal runout, then IT8 is achievable, so try it before you assume a reamer. Both statements are about a process, not a material miracle.
| Question | HSS jobber | Cobalt HSS | Solid carbide twist drill |
|---|---|---|---|
| Stiffness | Low | Low, same family as HSS | About 3× the modulus |
| Hot edge | Softens near 550–600°C | Better than plain HSS, still steel | Holds an edge much hotter |
| When it fails | Rubs, burns, goes oversize | Similar, usually later | Chips or snaps on impact |
| Best home | Low volume, forgiving setups | Portable and less rigid machines | Rigid CNC, true holder |
| Bolt-hole roundness | Often needs a second thought | Better life, same flex problem | Often good enough to drop the ream |
| Press fit / real H7 | No | No | No. Ream or bore |
IT widths below are the standard grades in ISO 286-1 for nominal sizes over 10 mm up to and including 18 mm. Other diameters use other rows. An H hole starts at zero and opens by this amount.
| Grade, 10 to 18 mm | Width | Typical route |
|---|---|---|
| IT7 (H7) | 0.018 mm | Ream or bore |
| IT8 (H8) | 0.027 mm | In range for a stable carbide drill, not guaranteed |
| IT9 (H9) | 0.043 mm | Common production result when the setup is honest |
| IT11 | 0.110 mm | Ordinary general-purpose drilling |
| IT12 | 0.180 mm | Wander, wear, or a plate that moved |
Do not take a single feed as “the” feed for every 8 to 16 mm carbide drill. Diameter, length-to-diameter, coolant, and the steel’s strength all move the number. The table below is one published baseline, not a Durable Mills lab result and not a universal law.
ISCAR’s solid-carbide drill recommendations for non-alloy steel under 0.25% carbon, annealed, about 420 N/mm2 and 125 HB, list a cutting speed of 80 to 120 m/min for diameters from 3 mm to 20 mm, with feed stepped by diameter. The same notes say to start in the middle of the range, keep radial and axial runout within 0.01 mm, cut the feed about 20% when length exceeds 6×D, and drop cutting speed about 10% if you have external coolant only.
| Drill diameter | Starting Vc | Starting feed | Source condition |
|---|---|---|---|
| 5.1 to 8 mm | 80–120 m/min | 0.15–0.25 mm/rev | ISCAR row: non-alloy steel, under 0.25% C, annealed, ~125 HB |
| 8.1 to 12 mm | 80–120 m/min | 0.20–0.30 mm/rev | Same row. Mid-band is the published place to start |
| 12.1 to 16 mm | 80–120 m/min | 0.20–0.35 mm/rev | Same row. Not a measured A572 trial |
| 16.1 to 20 mm | 80–120 m/min | 0.25–0.40 mm/rev | Same row. Reduce feed if the drill is longer than 6×D |
A36 often lives near that low-carbon group, but heats vary and scale is not in the table. A572 Grade 50 and S355 are stronger. Use the chart line for that strength, or ask us for the drill you actually bought. Starting at the middle and moving on the evidence of wear and chip is the instruction printed with the table. It is the right instruction.
Spindle speed:
n = (Vc × 1000) / (pi × D)
n is rev/min, Vc is m/min, D is mm. The inch form still taped to US machines: n = (SFM × 3.82) / diameter in inches. Feed speed is vf = n × fn. Time in the cut, with no peck and no air move, is depth divided by vf.
Worked arithmetic, not a stopwatch study. Take the middle of the ISCAR low-carbon band for a 12 mm drill: Vc = 100 m/min, fn = 0.25 mm/rev, through 25 mm.
n = (100 × 1000) / (pi × 12) = 2653 rev/min
vf = 2653 × 0.25 = 663 mm/min
25 / 663 minutes is about 2.3 seconds in the cut.
If an HSS drill were run at 30 m/min with the same feed per revolution, spindle speed and metal-removal time would scale with Vc, so the cut would take a bit over three times as long before anyone counts pecks. HSS in gummy A36 often does peck, because the flute packs. Each peck is another entry and another chance to mark the wall. That comparison is arithmetic from stated assumptions. It is not a cycle-time audit of a named cell, and it says nothing about tool life.
How to change the number without guessing:
A production carbide drill is a designed tool. Don’t stone a 140° split into a 118° “because the article said 118 is general purpose,” and don’t do the reverse on a drill whose web and flute were designed together. Use the mechanism to choose and to diagnose.
Point angle. A sharper point, around 118°, is easy to picture and leaves a wider disk of material at exit. A flatter point, often 135° to 140° on steel drills, shortens the chisel’s first contact on a flat face and leaves a smaller disk. Smaller disk can mean a smaller cap. It does not, by itself, mean a smaller burr. Exit support, feed through the last half millimetre, corner wear, and whether the plate dishes all move the crown. If two drills are identical except for point angle, the flatter point is the one we would try first on structural plate. If they are not identical, the point angle is one variable, not the result.
Split point and web. The web pushes. A thick web makes a strong drill and a high thrust. High thrust on a thin lug bells the part, and the hole goes out of round when the part springs back. A split or thinned web gives the center something that cuts, so thrust drops and the drill is less eager to walk. When a carbide drill “didn’t help,” unequal lips or a missing split are the first things we want to see, ahead of any argument about brand.
Margins and flutes. The margin has to guide without polishing. A shiny bore in A36 is usually rub. Double margins steer more and rub more; in sticky low-carbon plate a single margin with real body clearance is often the better trade until the hole is deep enough that extra guidance earns the friction. Helix near 30° is a normal steel choice because it lifts a long chip without making the outer corner fragile in scale. A packed flute ratchets. That ratchet is a lobe generator no coating will argue with.
Coating. TiAlN and AlCrN families are there for heat and for scale. On ten holes, lip match and runout matter more. On a few hundred, scale will round a bare corner and the burr comes back. Coating does not fix a grind error.
Back taper. Too little and the body rubs, torque climbs, and the wall looks torn partway down. Too much and the margins stop guiding once they leave the top of the hole. You tend to notice it only after a batch goes tight at mid-depth.
Sometimes. The decision is the hole’s job, not the drill’s marketing.
Structural bolting is loose on purpose. ANSI/AISC 360 Table J3.3 sizes standard holes larger than the bolt so the iron will erect. Through 1 inch bolts the usual standard hole is 1/16 inch over the bolt: 3/4 in a 13/16, 7/8 in a 15/16, 1 inch in a 1-1/16. Confirm the edition written on the contract before you detail from memory. If a bolt hangs in that hole, you are not “0.02 mm small.” You are lobed, burred, or both. A carbide drill that stays round, plus a chamfer if the print actually asks for one, is the process. A reamer is not adding quality. It is cleaning up a drill that wandered.
| The hole is for | Keep a reamer after a stable carbide drill? | Why |
|---|---|---|
| AISC-style bolt clearance | No | The allowance is already 1/16 inch. Round and deburred is the real requirement |
| Pin that falls in of its own weight | Usually no | Form and a small burr, not an H7 |
| Stack of plates for a through-bolt | No, if each hole is round | What is left is location, not a missing reamer |
| Slip bushing around H8 | Try without, then measure | IT8 is in the published carbide band only while runout and lips cooperate |
| Press fit or a true H7 pin | Yes, or bore | A drill, carbide included, is the wrong finishing tool |
| Cross-hole, weld, or a steep entry | Often yes, or a cleanup pass | The interruption chips corners and bruises form |
One fabricated-frame shop, mobile equipment, name withheld at their request, was reaming every 16 mm hole in 20 mm A572 Grade 50 brackets. The reamer was not holding a bearing fit. Fitters were using it to clear a lobed hole and a crown that snagged the pin. The change that stuck was a carbide drill, a fixture that clamped within about a diameter of the hole, and a runout check at the start of the shift rather than after a pallet felt wrong. The ream left that family of holes. A chamfer stayed, because a broken edge was on the print. Holes that broke into weld metal still got a finishing pass.
What this does not prove: we are not publishing a roundness trace, a before-and-after Cpk, a tool-life count, or a cycle-time study for that cell. Those would be the right next measurements if you are about to delete a ream on a part you cannot afford to scrap. Copy the clamp and the runout habit. Do not copy a hope that every 16 mm hole in Grade 50 will behave the same on a different machine.
Feed at exit matters as much as the tool. Keeping the feed up through breakthrough shears the cap. Easing off “to be gentle” often rolls a taller burr, because the last web bends. That is a mechanism, not a slogan: a cutting edge below a real chip load rubs, and rubbed ductile steel moves instead of separating. Support the exit. Do not dwell at depth. A dwell rubs a ring into the lip.



The 5D carbide drill by Durable Mills delivers exceptional centering accuracy and tool rigidity across demanding drilling operations. Engineered for cast iron, stainless steel, and alloy steels, this 5D carbide drill optimizes chip evacuation and heat resistance to increase CNC throughput. Choose our high-precision 5D carbide drill bits for stable hole tolerances and extended production runs.
The same mechanisms showed up in several sections above. One table is more useful than another five paragraphs that all end with “carbide cannot save a bad setup.”
| What you see | Likely cause | Check | Change |
|---|---|---|---|
| Hole oversize, round enough | Runout or one lip high | Indicator on the tool, compare the two lips | Holder, collet, or the grind. Do not just slow down |
| Mic passes, plug fails | Lobed form a two-point gauge missed | Plug, mating pin, or a roundness check | Clamp, stickout, lips, runout. Inspect form, not only size |
| Clean first holes, lobed later holes | Plate or stack started moving | Tap test, clamp distance, loose tacks | Clamp near the hole, bolt the stack, support the exit |
| Tall exit crown | Light feed at breakthrough, dull corner, no support | Watch the last 1 mm and the wear land | Keep feed through exit, replace a rounded corner, back the part |
| Corner chipped on hole one | Impact, not “A36 is too sticky” | Entry angle, exit pocket full of chips, weld, crash | Spot the face, clear the exit, slow only the interrupted part |
| Packed flute, torn wall | Depth, flute volume, coolant missing the point | Chips in the flute and where the stream actually hits | Shorter drill, through-coolant, or a feed the flute can carry |
| Tight halfway down | Body rub, little back taper, or scale pickup | Torque rise mid-hole, shine on the body | Tool geometry and speed, not a heavier feed |
Buy cobalt or HSS, and spend the money on fixtures, if any of these are true:
Punching still wins on thin plate in real volume when the edge is acceptable and no pin has to slip through. Carbide is for the middle: repetitive holes where roundness and a short cycle both matter, and the machine can support the tool.
When you order solid carbide twist drills for structural steel, match these to the print before you open the catalog:
Standard twist drills are the family we grind for this structural and alloy-steel work: a point and flute meant for a steel chip, in a body stiff enough to hold form when the setup does its half. If the diameter and length are already on the process sheet, the carbide twist drills page is the direct list. If they are not, send the print. Guessing “5/8 in steel” from a phone photo of a flange is how the wrong length gets ordered.
Send grade, not the word mild. Diameter, depth, through or blind. What passes through the hole. The hole roundness tolerance if it is written, or the gauge the fitter actually uses. Machine, holder, and the last runout someone measured. Flood, through-tool, or a bottle on a shelf. With that, a starting Vc and fn is a short conversation. Without it, any table in this article is a better education than a part number, and still not your process.
On AISC bolt holes, on many slip pins, and on stacks that only need a bolt to pass, a stable carbide drill often does. On H7 and on press fits, no. Sandvik and Kennametal’s published comments put IT8 in reach when runout is small and the part is still. They do not put a bearing fit in reach. Delete the reamer on the holes where you have measured form, not on every hole that shares a diameter.
Two flutes plus an orbit often cut an odd-lobed form, and a two-point mic reads across the high spots. Use a plug or the mating pin. Then check lip height, runout, stickout, and whether the plate moved. The triangle is a clue, not proof that every drilling error has three sides.
For ordinary structural bolting, specify the hole diameter from AISC Table J3.3 (or the EN rule on the job) and require the bolt to pass, burr controlled. That catches lobing without forcing an H7. For pins, write the fit you assemble to. Add a roundness value only after a two-point check has already shipped bad parts.
Use the chart for that drill. One published low-carbon baseline, the ISCAR row cited above, puts 12 mm in an 80 to 120 m/min band with about 0.20 to 0.30 mm/rev, starting mid-range, runout within 0.01 mm, on their geometry. At 100 m/min that is about 2650 rev/min. A572 Grade 50 is a stronger steel. Do not assume the same line. External coolant only, or a drill longer than 6×D, moves the number the way that chart’s notes describe.
Gummy A36 packs flutes and rolls burrs. It does not usually explode a corner on hole one. Look for a slap at entry, an exit into chips, runout loading one margin, or a weld the program ignored. Find the impact before you drop the speed into a rub.
Under about three diameters, in open plate, flood that reaches the point is usually enough. Deeper holes, and any pocket that refills with chips, are where through-coolant stops the tear. Air only is a compromise some beam lines live with. Tool life is the invoice.



Engineered for precision CNC drilling, our high-performance carbide twist drills deliver exceptional dimensional accuracy across cast iron, structural steel, and stainless steel. Featuring a 140° self-centering point geometry and wear-resistant PVD coating, these industrial carbide twist drills significantly enhance tool life in volume production. Durable Mills supplies premium straight shank carbide twist drills designed to minimize cycle times and machine downtime.
Keep it where the print is a real fit. Take it off where it only exists to clean up triangles and crowns, and only after the holder, the clamp, and the feed at exit are under control. A stiffer drill makes that possible. It does not make it automatic.
Send the print, the grade, and a photo of the hole that failed, lobed or crowned. We will say whether solid carbide twist drills for structural steel are the right cut, which length we would grind, and a starting speed taken from the drill you would actually receive, not from a generic midpoint. If cobalt or a reamer is the honest tool, that is the answer.
Ask on the contact page, or email info@durablemills.com. A picture of the bad hole is worth more than another paragraph about stiffness.